A segmental retaining wall is a stack of dry-cast concrete blocks holding back soil, and almost everything that decides whether it stands is buried before anyone sees the finished face: the leveling pad, the embedment depth, the gravel drainage column, and the compaction of the soil behind the units.

This is the construction side of that system. It covers what the block and geogrid details actually require in the field, in the order a crew builds them, and where the work most often goes wrong.

What a Segmental Retaining Wall Actually Is

Segmental retaining walls, usually shortened to SRW, are built from dry-cast concrete units that stack without mortar. Most systems use a lipped or pinned connection so each course sets back slightly from the one below, creating the batter that lets the wall lean into the slope it retains. NCMA guidance caps that batter at 20 degrees.

The units themselves are covered by ASTM C1372, Standard Specification for Dry-Cast Segmental Retaining Wall Units. That standard sets minimum unit properties, not wall capacity. The capacity comes from the system: unit mass, the connection between courses, the geogrid where it is used, the drainage, and the soil that is compacted behind the face.

That is why a wall built to the drawing with the wrong backfill or a missing drain still fails. The block is the visible part of an engineered assembly, and the assembly is what carries the load.

The Leveling Pad Decides the Wall

Every SRW starts on a leveling pad, and the pad is where small errors get magnified over the height of the wall. NCMA recommends a minimum pad thickness of 6 inches, and a pad width at least 12 inches greater than the depth of the face unit so there is working room on both sides. The material is either densely compacted gravel or unreinforced, low-strength concrete, depending on the system and the spec.

The trench is excavated to the pad thickness plus the required embedment, then compacted to the density called for in the geotechnical report and inspected before any units go down. NCMA is blunt about the consequence of skipping that step: if the pad is not level when the units are installed, the finished wall will not be level.

On grade changes, the pad steps rather than slopes. Each step-up has to hold the required embedment at its own elevation, and the base material at the end of each step needs extra compaction because that corner carries the transition. If the foundation soil is soft, no amount of careful block setting will fix it — see soil stabilization for unstable subgrade.

Embedment: How Much Wall Goes Underground

Embedment is the buried height below finished grade at the toe, and it is the resistance that keeps the wall from sliding out or kicking forward. For level ground, the NCMA minimum is 6 inches to the top of the leveling pad. The bottom of the wall should not sit above finished grade measured 4 feet in front of the face.

When the ground in front of the wall slopes away, the required embedment increases. NCMA's guidance uses a fraction of the exposed wall height: roughly one-twentieth of the exposed height where the toe slope falls at 3H:1V, and one-tenth where it falls at 2H:1V. Abutment conditions use similar but deeper fractions. Toe slopes, high surcharges, and any chance of scour at the base all push the embedment deeper again.

Walls with a slope below them also need additional buried courses, and they generally need a global stability check by an engineer. That is the analysis that asks whether the whole hillside moves, not just the wall.

Gravity Walls and Geogrid-Reinforced Walls

Short walls often work as gravity structures: the mass of the units and the width of the base resist the soil pressure, and the manufacturer's design chart gives a maximum height for the soil and loading conditions. Taller walls, walls under surcharge, and walls with a slope above them are usually reinforced.

In a reinforced SRW, layers of geogrid are placed between courses and extend back into a compacted soil mass. The grid ties the face to that mass, so the wall behaves as a much wider, heavier structure. NCMA's minimum reinforced zone is 60 percent of the wall height for the bottom and middle layers and 90 percent of the height for the upper layers.

The vertical layout matters as much as the length. The first geogrid layer goes on top of the first or second course, and the top layer should be no deeper than two courses plus the cap, or 24 inches. Maximum spacing is generally 16 inches, and it should never exceed 24 inches even where the design allows wider spacing.

Grid is directional. The strong axis runs perpendicular to the wall face, the roll is laid flat and taut with no wrinkles, and it is placed at the elevation shown on the drawings. If you are new to the material, the difference between a geogrid and a fabric is covered in geogrid and geotextiles explained.

The Reinforced Soil Zone and What Goes In It

The soil behind the wall is a structural material, and it has a specification. NCMA recommends well-graded and poorly graded gravels and sands, plus silty gravels and sands, with the gradation and plasticity values set in the design. Soils classified as highly plastic or organic — MH, CH, OH, OL, and PT — are not recommended for any segmental retaining wall construction.

There is a limited exception for lower walls. A clayey sand classified SC can be used below 10 feet of height when the plasticity index is under 20 and the liquid limit is under 40, provided the wall has proper internal drainage including the gravel fill column.

Every soil behaves differently at optimum moisture, which is why the geotechnical report matters. It provides the strength and weight parameters the design was run against, and the fill placed in the field has to match them. A wall designed on a granular fill and built with on-site clay is not the same wall.

Gravel Fill and Drainage Behind the Wall

Behind the block face, the wall needs a drainage column of free-draining gravel — a clean, no-fines stone such as a #57. NCMA calls for a minimum of 12 inches of gravel fill behind the block, with a combined unit and gravel fill thickness of at least 24 inches.

Filter fabric separates that gravel from the retained soil and from the topsoil at the surface, so fines do not wash into the stone and clog it. A perforated drain pipe sits at the base of the column and runs to daylight. Some wall details also include a heel drain at the back of the reinforced zone.

At the top of the wall, the detail is just as important. Swales behind the wall carry surface water away so it never flows over the cap and down the face, and the finish grading typically uses a low-permeability layer under topsoil to shed water rather than let it soak straight down into the reinforced zone.

Water is the most common reason a block wall bulges, and the drainage detail is what controls it. If you want the reference for stone sizes and gradations, see gravel and stone sizes explained and building a drainage swale.

Compaction: The Part Everyone Rushes

NCMA recommends compacting the entire reinforced soil zone to at least 95 percent of standard Proctor density under ASTM D698, or 92 percent of modified Proctor under ASTM D1557. Moisture should be within about two percentage points of optimum, though every soil behaves differently and the geotechnical engineer's direction governs.

Lifts are limited to 8 inches compacted, or one course of block, whichever is less. Where a slope sits above the wall, that slope soil gets the same compaction effort as the retained soil, because it is part of the same load.

Equipment choice matters near the face. A large vibratory roller working tight to the block will push the units out of line, so most crews use a walk-behind plate or rammer within a couple of feet of the face and keep the heavy roller back in the reinforced zone. The trade-off between plate compactors, rammers, and rollers is covered in choosing the right compaction equipment.

Density testing is scheduled by course at varying locations across the reinforced zone, not just at one convenient spot. One passing test near the access point says very little about the back of the grid.

Building the Wall, Course by Course

The sequence is straightforward but unforgiving. Set the line and grade, string the batter, and bed the first course fully on the pad, level along the wall and across its depth. Every course after that starts by sweeping the top of the previous one clean so grit does not hold the units apart.

Geogrid goes in at the elevations shown on the drawings, with the specified embedment into the face unit and the strong direction running back into the slope. Gravel fill rises with the wall. Backfill is placed and compacted in lifts, and the crew keeps soil from spilling over the face as the wall goes up.

At the top, cap units finish the wall. NCMA's construction tolerance is tight: the variation between two points along the wall should not exceed 1 percent of the distance between them. A wall that wanders visibly over its length is usually a pad or line problem that was never corrected early.

When the Wall Needs an Engineer

Some walls can be built from a manufacturer's chart and a standard detail. Others cannot, and the triggers are well defined. A slope above or below the wall, clay, silt, poorly graded sand or expansive clay in the foundation, shallow groundwater at the face, or a significant surcharge all call for a global stability analysis.

Terraced walls, walls in water applications, and walls carrying fences or guardrails also need design attention. A fence post set too close to the face can compromise the grid, so posts are usually held at least 3 feet back from the face or set in sleeves installed during construction so no excavation is needed afterward.

Local codes can be stricter than industry guidance, and taller walls commonly require a sealed design and a permit. The permit side is covered in excavation and grading permits, and the soil investigation behind the design in what is a geotechnical report.

Common Failures and a Pre-Backfill Checklist

Most SRW failures fall into a few patterns. Bulging and leaning come from saturated backfill with a blocked or missing drain. Settlement comes from uncompacted fill or a soft foundation that was never evaluated. Face rotation comes from geogrid that was too short, placed at the wrong elevation, or tied into soil that did not match the design.

Before backfill covers the work, walk the wall and confirm the following:

  • The leveling pad is level, at least 6 inches thick, and wide enough on both sides of the unit.
  • Embedment matches the drawing at every station, including at step-ups.
  • The gravel column is at least 12 inches behind the face, clean stone, with filter fabric on the soil side.
  • The drain pipe is at the base, sloped, and discharges to daylight.
  • Every geogrid layer is at the right elevation, the right length, flat, and undamaged.
  • Compaction tests are passing through the full reinforced zone and moisture is near optimum.
  • Surface water has a swale or grade path that keeps it away from the top of the wall.

Block walls are one option among several. If stone-filled baskets suit the site better, compare the details in gabion walls, and for the excavation side of the base trench see excavating for a retaining wall.

Matt

Matt

Excavation Expert

Matt is a highly experienced heavy equipment operator with over two decades of experience in the construction industry. His expertise covers a wide range of machinery and project types, and he is known for his focus on safety, efficiency, and problem-solving. Matt's commitment to delivering high-quality work within deadlines and budgets has made him highly respected at Centex Excavation and the excavation industry.

We may be compensated through the links you find on this page.

Join the List!

Sign up for the CEX Insider and get the latest in the excavation industry delivered right to your inbox!
Don't worry, we will never spam you.

Latest from CEX


Trending